China Nickel Based Superalloy Hastelloy C276 Strip UNS N10276 China Nickel Based Superalloy Hastelloy C276 Strip UNS N10276 China Nickel Based Superalloy Hastelloy C276 Strip UNS N10276

Nickel Based Superalloy Hastelloy C276 Strip UNS N10276

MOQ: 5 Kg
Price: 50 - 999 kilograms US$55.00
PRODUCT DESCRIPTION
Payment Terms L/C, T/T, Western Union, MoneyGram
Supply Ability 300 tons per month
Delivery Time 7 to 20 Days
Packaging Details Plastic film or waterproof woven bag inside, wire packed in spool put into carton,coil wire or strip wire put into wooden case
View More
ABOUT US
China factory - Changzhou Victory Technology Co., Ltd
Changzhou Victory Technology Co., Ltd
Jiangsu , China
5.0
Verified Supplier
View More
GET THE BEST PRICE FOR
China Nickel Based Superalloy Hastelloy C276 Strip UNS N10276
Nickel Based Superalloy Hastelloy C276 Strip UNS N10276
MOQ: 5 Kg
Price: 50 - 999 kilograms US$55.00
Continue
RECOMMENDED PRODUCTS
ABOUT US
China factory - Changzhou Victory Technology Co., Ltd
Changzhou Victory Technology Co., Ltd
Jiangsu , China
5.0
Verified Supplier
Company Name Changzhou Victory Technology Co., Ltd
Business Type Manufacturer,Distributor/Wholesaler,Trading Company,Seller
Brands Victory
Employee Number 100~150
Year Established 2008
Total Sales Annual 100-100000
Company Location NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu
Factory Location NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu
Get Latest Price for your requirement
PRODUCT DESCRIPTION