Find The Best Chinese Factory
Alloy Type | Cobalt-based Reinforced Superalloy |
Equal Grade | UNS N10276, Hastelloy C276, |
Raw Materials | NI Rem%, CR20-22.5%, MO12.5-14.5% |
Yield Strength | 350 MPa |
Company Name | Changzhou Victory Technology Co., Ltd |
Business Type | Manufacturer,Distributor/Wholesaler,Trading Company,Seller |
Brands | Victory |
Employee Number | 100~150 |
Year Established | 2008 |
Total Sales Annual | 100-100000 |
Company Location | NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu |
Factory Location | NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu |